Heat-Shrinkable-Anti-Tracking-Straight-Boot

Technical Data:

Property Requirements Test Method
Tensile Strength 8N/mm2 (min.) ASTMD 412, ESI09-13
Elongation 200% (min) ASTMD 412, ESI09-13
Heat Aging
(500 hrs. at 1200 C)
   
Tensile Strength 7N/mm2 (min.) ASTMD 412
Elongation 200% (min.) ASTMD 412
Cold Temperature
Flex (-400 C)
No cracking ASTMD 2671
Electrical    
Dielectric Strength
10 kV/mm (min.) ASTMD 149, IEC 243
Volume Resistivity 1 x 1012 ohm-cm (min.) ASTMD 257
Track Resistance Non-Tracking ASTMD 2303
Chemical Resistance    
Tensile Strength 7N/mm2 (min.) ASTMD 412
Elongation 200% (min.) ASTMD 412

Dimension Chart

Code Expanded Recovered Recovered P±10%  
Ø H (max.) Ø J(min.) Ø H (max.) Ø J(min.)
DSB - 1 80.0 34.0 32.0 19.0 225.0
DSB - 2 80.0 58.0 32.0 29.0 225.0

Enquiry New !